There are Korean imported diamond, Taiwan import, domestic film, domestic acrylic, Austrian, Czech. South Korean imported drill: high brightness, no variegated chip drill.

The cutting surface or spherical surface is uniform, the color is uniform, the defective rate is between 0.5% and 1%. The probability of degum is 0% to 1%, not fading, and the fastness is high.

Back to pale green, 10 aspects, lead content is about 5%, the temperature is about 120 degrees when ironing, comprehensive defect rate is 3% - 5%, after years of market validation, quality is reliable, has good washing fastness, color pure, uniform cutting, low prices, for the mainstream market products.

Taiwan imports: high brightness, no variegated film, uniform cut surface or spherical surface, uniform color uniform, the defective rate is between 1% and 3%, the probability of taking off the base is 0.5%-0.8%, not fading, and the firmness is high.

Domestic film: low brightness, mixed color film, cut surface or spherical surface uneven, uneven color, the defective rate is 3%-10%, the probability of degum is 1%-5%, will fade, the firmness is low.

The back is dark green, 8 cut products, no lead, and the ironing temperature is 80 degrees. The defective rate is very high, the fastness is poor, the color has the deep and shallow phenomenon, because its price is low, has a certain market share, the main application is in the mass-produced clothing.

Domestic acrylic: strictly speaking, acrylic is not a diamond, but a product between plastic and glass. Good brightness, poor firmness, hot drilling temperature should not be too high, if more than 80 degrees, may cause the pressure to melt. Often used in low-grade children's clothing.

Austria drill: short for short - auger, high brightness, no variegated drill, uniform cutting surface, uniform color, the defective rate is 0.01%-0.02%, the gum is grey.

There are 14 cutting, 12 cutting and 8 cutting products, 12 of which are now out of production, and the 8 cut products are only white and white.

The color and specifications of the products are complete. The quality of the material is 30%, the temperature of the hot drill is 175 degrees, the comprehensive defect rate is 3-5%, the quality is excellent, it is firm and reliable, and can be washable and dry-cleaned. But the price is high, belong to non - mainstream market product.

The Czech drill: high brightness, no noise, uniform cut surface, uniform color, defect rate from 0.01% to 0.02% of the finest hot drilling, warm wool, elegant design, magnificent, very hot drill and sweater jointly interpret fashion.

The gum is transparent and has bubbles. For the 8 cut products, the lead is 25%, the ironing temperature is 140 degrees, the comprehensive defect rate is 3% to 5%, the quality is good, the price is second only to the auger, it belongs to the mainstream market products.